Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet

Category Polymer , Thermoset , Melamine , Melamine Formaldehyde, Molded, Glass Fiber Filler
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 2.00 g/cc
1.70 - 2.00 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 150 MPa
>= 21800 psi
IEC 1212-2 5.7
Flexural Strength >= 240 MPa
>= 34800 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 14.0 GPa
>= 2030 ksi
IEC 1212-2 5.2
Compressive Strength >= 275 MPa
>= 39900 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 60.0 MPa
>= 8700 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 31.0 kJ/m²
>= 14.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 3.00 J/cm²
>= 14.3 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
IEC 1212-2 7.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+8 ohm
>= 1.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 7.5

@Frequency 48.0 - 62.0 Hz
<= 7.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 7.5

@Frequency 1.00e+6 Hz
<= 7.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 15000 V

@Temperature 90.0 °C
>= 15000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.020

@Frequency 48.0 - 62.0 Hz
<= 0.020

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.020

@Frequency 1.00e+6 Hz
<= 0.020

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 500 V
>= 500 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Proof Tracking Index 500
IEC 1212-2 6.4
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 414 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm
Copyright © lookpolymers.com All Rights Reserved