Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 15000 V | 15000 V | |
Saint-Gobain CHR® 2255-5 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 15000 V | 15000 V | |
Saint-Gobain CHR® 2265-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | >= 15000 V | >= 15000 V | IEC 626 |
Dr. D. Mueller Flexiso® DMD FI 14010 00310 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00310 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Dielectric Breakdown | >= 15000 V @Temperature 90.0 °C |
>= 15000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 15000 V @Temperature 90.0 °C |
>= 15000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Dielectric Breakdown | 15000 V | 15000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |