Polymer Property : Tensile Strength = 300 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 300 MPa

@Thickness >=1.60 mm
43500 psi

@Thickness >=0.0630 in
EN 60893
HOS-Technik Homide 250 Bismaleimide Resin
Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel..
Tensile Strength 300 - 400 MPa
43500 - 58000 psi
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat..
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information..
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret..
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..