Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 300 MPa @Thickness >=1.60 mm |
43500 psi @Thickness >=0.0630 in |
EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |
|||
Tensile Strength | 300 - 400 MPa | 43500 - 58000 psi | |
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat.. |
|||
Tensile Strength | >= 300 MPa | >= 43500 psi | IEC 1212-2 5.7 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Tensile Strength | >= 300 MPa | >= 43500 psi | IEC 1212-2 5.7 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Tensile Strength | >= 300 MPa | >= 43500 psi | IEC 1212-2 5.7 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Tensile Strength | >= 300 MPa | >= 43500 psi | IEC 1212-2 5.7 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Tensile Strength | >= 300 MPa | >= 43500 psi | IEC 1212-2 5.7 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |