Electrical Properties Metric English Comments
Insulation Resistance 5.00e+10 ohm
5.00e+10 ohm
Wet; 24 hours in water; IEC 167
Vyncolit X613 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller..
Insulation Resistance 5.00e+10 ohm
5.00e+10 ohm
Wet; 24 hours in water; IEC 167
Vyncolit 2723 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre..
Insulation Resistance >= 5.00e+10 ohm
>= 5.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information..
Insulation Resistance >= 5.00e+10 ohm
>= 5.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret..
Insulation Resistance >= 5.00e+10 ohm
>= 5.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Insulation Resistance >= 5.00e+10 ohm
>= 5.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..