Heatbath/Park #50 Oil Quench

Category Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park #50 Oil Quench.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low viscosity quench oil that approaches water in quench speed, yet gives a more uniform, less severe quench than water. Recommended for open quench system operating below 120°C.Information provided by Heatbath Corporation - Park Metallurgical.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 45 SUS
45 SUS
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 48.9 °C
120 °F
Upper limit of working range
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Lower limit of working range
Flash Point 138 °C
280 °F