Material Notes:
SOLKAFLAM® 125 UL - recognized component fire extinguishing agents CAS-No.: 354-33-6 / EC-No.: 206-557-8 / REACH Registration Number: 01-2119485636-25 Uses: Fire extinguishing agentInformation provided by Solvay
Physical Properties Metric English Comments
Molecular Weight 120 g/mol
120 g/mol
Thermal Properties Metric English Comments
Melting Point -103 °C
-153 °F
Boiling Point -48.5 °C

@Pressure 0.1013 MPa
-55.3 °F

@Pressure 14.69 psi
Descriptive Properties Value Comments
Appearance compressed liquefied gas
Color colorless
Composition >99.5%
Pentafluoroethane