Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 48.9 °C | 120 °F | |
Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump effi.. |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure Liquid, Grey Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | Upper limit of working range |
Heatbath/Park #50 Oil Quench Low viscosity quench oil that approaches water in quench speed, yet gives a more uniform, less severe quench than water. Recommended for open quench system operating below 120°C.Information provi.. |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 48.9 °C | 120 °F | |
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl.. |