Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | 50% relative humidity |
Chesterton 763 Rust Transformer® Description: Chesterton® 763 Rust Transformer® is a mild, natural acid based product which electrochemically transforms rust into a corrosion inhibiting protective film. It is the labor saving way.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000-77 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Dry, flat surfaces without rivets |
3M Scotchcal™ 5000 Reflective Graphic Film' 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity w.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-96 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-10 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-105 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | flat surfaces without rivets |
3M Scotchlite™ 680-81 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7218SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curves or corrugations with rivets |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Safety-Walk™ 280 White Slip-Resistant Fine Resilient Tapes and Treads A fine-textured, slip-resistant surface with a pressure-sensitive adhesive backing provides enhanced safety and comfort in light- and barefoot- traffic areas. For wet, barefoot-traffic areasNon-mine.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000-14 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-139 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-39 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-54 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-64 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-98 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-24 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-46 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ IJ65 Perforated Window Graphic Film Film IJ65 is an intermediate, 6-mil vinyl film with a 50% die-perforated pattern and a removable, pressure adhesive. This film allows a full image to be seen on the outside of a window while allowin.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7940 Aluminum Foil Label Material 3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 180 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000LF-12 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |