Material Notes:
Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in various motor, transformer, coil, and other applications requiring low hysteresis or magnetic flux losses.Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 3.28 g/cc
3.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Barcol 35 - 40
35 - 40
ASTM D2583
Flexural Strength 112.4 MPa
16300 psi
LW; ASTM D790
123.6 MPa
17920 psi
CW; ASTM D790
Flexural Modulus 6.052 GPa
877.8 ksi
LW; ASTM D790
6.716 GPa
974.1 ksi
CW; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 23.8 µm/m-°C
13.2 µin/in-°F
ASTM D696-08
Specific Heat Capacity 0.6434 J/g-°C
0.1538 BTU/lb-°F
ASTM E-1269-05
Thermal Conductivity 0.717 W/m-K
4.98 BTU-in/hr-ft²-°F
ASTM E-1925-06
Maximum Service Temperature, Inert 155 °C
311 °F
IEEE
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
ASTM D257