Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.28 g/cc | 3.28 g/cc | ASTM D792 |
Haysite H208 Polyester, Magnetic Permeable Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari.. |
|||
Specific Gravity | 3.28 - 3.31 g/cc | 3.28 - 3.31 g/cc | ASTM D792 |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |