Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 155 °C | 311 °F | IEEE |
Haysite H208 Polyester, Magnetic Permeable Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari.. |
|||
Maximum Service Temperature, Inert | 155 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
311 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Maximum Service Temperature, Inert | 155 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
311 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Maximum Service Temperature, Inert | 155 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
311 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Maximum Service Temperature, Inert | 155 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
311 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |