H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 10 - 14 µm
10 - 14 µm
10%
15 - 17 µm
15 - 17 µm
50%
16 - 18 µm
16 - 18 µm
MV
28 - 41 µm
28 - 41 µm
90%
62 µm
62 µm
Minimum of 98% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 3.5 - 4.5 %
3.5 - 4.5 %
Chromium, Cr 3.0 - 5.0 %
3.0 - 5.0 %
Cobalt, Co 8.5 - 11.5 %
8.5 - 11.5 %
Iron, Fe <= 0.80 %
<= 0.80 %
Oxygen, O <= 0.20 %
<= 0.20 %
Tungsten, W 78 - 85 %
78 - 85 %