Polymer Property : Particle Size = 14 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 7.0 - 14 µm
7.0 - 14 µm
average
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Particle Size 7.0 - 14 µm
7.0 - 14 µm
average
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Particle Size 8.0 - 14 µm
8.0 - 14 µm
average
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarThermâ„¢'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Particle Size 1.6 - 14 µm
1.6 - 14 µm
d10
Indium Corp. In(OH)3 Crystalline Indium Hydroxide
Indium Acetate is a white powder. Crystalline Form: Primary particles range from 1 to 5 microns in size. They are cubic in shape and form agglomerates up to approximately 35 microns.PropertiesChe..
Particle Size 10 - 14 µm
10 - 14 µm
10%
H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 10 - 14 µm
10 - 14 µm
d90, Guaranteed
TIMCAL TIMREX® PP 10 Natural Flake Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 8.0 - 14 µm
8.0 - 14 µm
average
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen..