Polymer Property : Particle Size = 41 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 35 - 41 µm
35 - 41 µm
MV
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 34 - 41 µm
34 - 41 µm
50%
H.C. Starck Amperit® 109.066 Agglomerated Sintered Molybdenum (Mo)
Particle Size 28 - 41 µm
28 - 41 µm
90%
H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 33 - 41 µm
33 - 41 µm
50%
H.C. Starck Amperit® 584.1 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)