Physical Properties Metric English Comments
Particle Size 28 µm
28 µm
median; Microtrac
Nyco NYAD® MG Wollastonite
High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct..
Particle Size 28 - 32 µm
28 - 32 µm
90% finer than
Potters Industries Sphericel® 60P18 Hollow Glass Spheres
Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive..
Particle Size 28 µm
28 µm
Method C; Internal Method
Solvay Specialty Polymers Halar® 3404DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Halar® 3404DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug and Cosmetic Act food additive regulation ..
Particle Size 28 µm
28 µm
Method C; Internal Method
Solvay Specialty Polymers Halar® 9414 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&l
Halar® 9414 is a filled, pearl-white, semicrystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and can be used as a primer, intermediate or topcoat in pr..
Particle Size 28 - 34 µm
28 - 34 µm
50%
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10
Particle Size 28 - 38 µm
28 - 38 µm
50%
H.C. Starck Amperit® 539.054 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt-Chromium (WC-WB-Co-Cr) 60-30-5-5
Particle Size 28 - 34 µm
28 - 34 µm
50%
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr)
Particle Size 28 - 35 µm
28 - 35 µm
50%
H.C. Starck Amperit® 140.3 Tungsten (W)
HS Number: 81011000
Particle Size 28 - 35 µm
28 - 35 µm
50%
H.C. Starck Amperit® 146.3 Chromium (Cr)
HS Number: 81122031
Particle Size 28 - 41 µm
28 - 41 µm
90%
H.C. Starck Amperit® 553.065 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 28 - 36 µm
28 - 36 µm
50%
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 28 µm
28 µm
Silberline SilBerCote® 3500-20Y
SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add..
Particle Size 28 µm
28 µm
Silberline Sparkle Silver® 3000-AR
Sparkle Silver® 3000-AR is a medium, high sparkle, brilliant, non-leafing aluminum pigment popular for solvent Automotive Applications. It shows exceptional resistance to spotting when incorporat..
Particle Size 28 µm
28 µm
Silberline Sparkle Silver® 3201-ST
Sparkle Silver® 3201-ST is finer in particle size than Sparkle Silver® 3141-ST, and has improved hiding properties. It is a non-leafing aluminum pigment, has brilliant sparkle, and is controll..
Particle Size 28 µm
28 µm
@ 98%
CIMBAR CLEAR-BLOC® 80 Antiblock Talc
CLEAR-BLOC® 80 talc, produced from high purity ore provides high brightness, clarity, low iron content and low surface area for primary use as an anti-block additive in LDPE and LLDPE film applicat..
Particle Size 28 - 32 µm
28 - 32 µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 2002 ES 3 Nat 3 Polyamide 12
Information provided by Arkema Group
Particle Size 28 - 38 µm
28 - 38 µm
D(0.5)
Akzo Nobel Expancel® 093 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 28 - 38 µm
28 - 38 µm
D(0.5)
Akzo Nobel Expancel® 930 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 28 µm
28 µm
90" Percentile
3M W-610 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Particle Size 28 - 38 µm
28 - 38 µm
D(0.5)
Akzo Nobel Expancel® 092 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 28 - 38 µm
28 - 38 µm
D(0.5)
Akzo Nobel Expancel® 950 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 28 µm
28 µm
Before Conversion
Silberline Sparkle Silvet® 880-20-J
Sparkle Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pig..