Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is a screen printable polymer paste designed as a counter electrode in electrochemical biosensors. This ink can be used in conjunction with our working carbon electrode ink C2030519P4, to increase the conductivity of the carbon by printing tracks underneath.Low silver contentScreen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-325tpiSubstrate: Polyimide, PET, PENInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 44 - 46 %

@Temperature 700 °C
44 - 46 %

@Temperature 1290 °F
Viscosity 900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.015 - 0.020 ohm

@Thickness 0.0250 mm
0.015 - 0.020 ohm

@Thickness 0.000984 in
Printed onto 125 µm PET film
0.030 - 0.045 ohm

@Thickness 0.0100 mm
0.030 - 0.045 ohm

@Thickness 0.000394 in
Printed onto 125 µm PET film
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
belt dryer
10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
15.0 min

@Temperature 135 °C
0.250 hour

@Temperature 275 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 250-270
Using a 230 mesh stainless steel screen