Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DIOFAN® A 736 is a PVDC latex used as a flexible underlayer for coating on paper, cardboard and rigid PVC foils, to be covered with an appropriate topcoat.Features: Good Flexibility; Moisture Barrier; Oxygen BarrierUses: Barrier Coatings; Coating ApplicationsAdditional Properties: Ball Drop Test - > 900 mm; Density - 1.300 g/cm³; Density - 1.650 g/cm³; Emulsion Type - Anionic; Filmability - 17 °C; Oxygen Transmission Rate - ASTM D3985 21 cm³/m²/bar/24 hr; pH - 2.5; Shelf Life - (23°C): 12 month; Solids Content - 600 g/kg; Surface Tension - 45 mN/m; Viscosity - (20°C): 20 mPa·sInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 18.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
1.16 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Tensile Impact Strength 500 kJ/m²
238 ft-lb/in²
ASTM D1822
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings DMF 11383; EC 1907/2006 (REACH); EU No 10/2011
FDA 21 CFR 176.170; FDA 21 CFR 176.180
Availability Asia Pacific
Europe
Latin America
North America
Form Liquid