Physical Properties Metric English Comments
Viscosity 900 - 1100 cP
900 - 1100 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 160 LOW ODOR/LOW BLOOM (1000 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PAA-033 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-031 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-052 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-055 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-058 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-064 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PPA-019 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PNA-157 Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP
700 - 1100 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1163 B (SIS) Linear Block Copolymer
Description: Kraton D1163 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra..
Viscosity 900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste
This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be ..
Viscosity 700 - 1100 cP
700 - 1100 cP
Huntsman PY 258 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 185 to 196. Max color is 3.Comments/Applications: Provides excellent heat and chemical resistance especially in post bake or heat cured coatings. Chemically modified..
Viscosity 700 - 1100 cP
700 - 1100 cP
Beijing Ranger Chem SM-815 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 700 - 1100 cP
700 - 1100 cP
Beijing Ranger Chem WSR615 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
900 - 1100 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste