Gwent Electronic Materials C2070508D4 Carbon Graphite Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2070508D4 Carbon Graphite Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Carbon Graphite Ink is designed to be used for screen printing working electrodes. These electrodes enable the detection of many analytes when used in conjunction with peroxidase and other oxidase type enzymes. The ink contains Potassium Ferrocyanide a mediator that makes the electrodes suitable to use with Horseradish Peroxidase for hydrogen peroxide (H2O2) detection. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 39 - 43 %

@Temperature 130 °C
39 - 43 %

@Temperature 266 °F
Viscosity 3500 - 4500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 4500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 29.71 microns
1.170 mil
Cured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 46.28 ohm

@Thickness 0.0250 mm
46.28 ohm

@Thickness 0.000984 in
Printed through 230 stainless steel mesh with 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 80.0 °C
0.250 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 280.5
Using a 230 mesh stainless steel screen