Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental and abrasion resistance with good flexibility and adhesion to alternative ITO coated substrates.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use to ensure complete homogeneity.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 54.9 - 55.1 %
54.9 - 55.1 %
Viscosity 6000 - 10000 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
6000 - 10000 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer with the PK1.1°
Thickness 16.0 - 18.0 microns
0.630 - 0.709 mil
Cured film
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.055 ohm
<= 0.055 ohm
at 25 microns thick
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
10.0 min

@Temperature 130 °C
0.167 hour

@Temperature 266 °F
box oven
Shelf Life 3.00 Month
3.00 Month
at 20°C maximum
6.00 Month
6.00 Month
at 5°C maximum
Descriptive Properties Value Comments
Coverage cm2/g 200
230 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens