Physical Properties Metric English Comments
Viscosity 6000 cP
6000 cP
A
NuSil MED-6215 Low Consistency Elastomer - Unrestricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Viscosity 6000 cP

@Temperature 190 °C
6000 cP

@Temperature 374 °F
melt viscosity; ASTM D 3236
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO)
Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding ..
Viscosity 6000 - 8000 cP
6000 - 8000 cP
ND Industries StudGrade® 137 Permanent HT Threadlocker
General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required.
Viscosity 6000 cP
6000 cP
Part B, RVT, #6, 20 rpm; TM R050-12
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Viscosity 6000 cP
6000 cP
mix viscosity
Aremco Aremco-Bond™ 855 Epoxy Adhesive  (discontinued **)
High performance epoxy for specialty bonding and potting applications to 350ºF (175°C). Can be applied to a myriad of substrates, offering exceptional chemical, electrical, and mechanical properti..
Viscosity >= 6000 cP
>= 6000 cP
NuSil Lightspan™ LS-3351 Silicone Optical Gel
General Purpose: Optical GelsComments: Use with Phosphor, Index matches to Crown Glass such as BK7, Index matches to plastics such as COCApplications: Excellent for Dispersing PhosphorInformation pr..
Viscosity 6000 - 40000 cP
6000 - 40000 cP
Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 233 to 278. Max color is 3.Comments/Applications: GY 6040 - 90% solids in xylene. General purpose bis A epoxy solution for use in 2-package maintenance and architect..
Viscosity 6000 - 40000 cP
6000 - 40000 cP
Huntsman Araldite GZ 6097 PM-55 Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 2000 to 2500. Max color is 3.Comments/Applications: GZ 6097 - 55% solids in PM (propylene glycol monomethyl ether). Much higher flexibility and toughness than GT 707..
Viscosity 6000 - 16000 cP
6000 - 16000 cP
Huntsman AroCy XU 71787.07 L Cyanate Ester
Comments/Applications: Toughened Dicyclopentadiene based cyanate ester resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Viscosity 6000 cP
6000 cP
Mixed Viscosity
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black
Information provided by ITW Devcon
Viscosity 6000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
6000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials D50706D2 Polymer Dielectric
This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode..
Viscosity 6000 cP
6000 cP
Shin-Etsu Silicones KE-1204 A Silicone, Potting/Encapsulation RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity <= 6000 cP
<= 6000 cP
#3 SP @ 12 rpm
Solvay MACKADET® DR-100M Surfactant
Product Description: Mackadet® DR-100M is a concentrated blend of surfactants, which simply requires dilution and the addition of minor additives to produce a ready to package high foaming produc..
Viscosity <= 6000 cP
<= 6000 cP
#3 SP @ 12 rpm
Solvay MACKADET® EQ-112 Surfactant
Product Description: Mackadet EQ-112 is mild blend of ingredients for the formulation of tear-free baby shampoos. Dilution at 27% in water gives a standard baby shampoo. Uses: Foam Pump, Bubble Bath..
Viscosity 6000 - 7000 cP

@Temperature 23.0 °C
6000 - 7000 cP

@Temperature 73.4 °F
Master Bond EP41S-1 Chemically Resistant Two Component Epoxy System
Master Bond Polymer System EP41S-1 is a two component epoxy resin system designed for durable, high performance bonding, sealing, coating and encapsulating. It successfully withstands prolonged imm..
Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Cast F353 Optically Opaque Casting System
TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical..
Viscosity 6000 - 10000 cP

@Temperature 23.0 °C
6000 - 10000 cP

@Temperature 73.4 °F
Master Bond UV15-7LRI One Component, Optically Clear UV Curable System
Master Bond Polymer System UV15-7LRI is a one component, optically clear, non-yellowing UV curable polymer system for high performance adhesives, sealants and coatings. When exposed to a source of U..
Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive
TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c..
Viscosity 6000 - 9000 cP

@Temperature 20.0 °C
6000 - 9000 cP

@Temperature 68.0 °F
DIN EN ISO 3219
Evonik Corporation POLYVEST® OC 800 S Polybutadiene
POLYVEST OC 800 S is a maleic anhydride adduct of a low molecular weight cis-1.4-polybutadiene. This polybutadiene adduct has succinic anhydride groups randomly distributed along the polymer chains...
Viscosity 6000 - 10000 cP

@Temperature 190 °C
6000 - 10000 cP

@Temperature 374 °F
melt, rotational viscometer; DIN 53 019
Evonik Corporation VESTOPLAST® 308 Amorphous Polyalphaolefin
VESTOPLAST 308 is a functionalized, amorphous polyalphaolefin, and butene-rich. Generally used as hot melt adhesives with good adhesion to metal and polar substrates.
Viscosity 6000 - 10000 cP

@Temperature 190 °C
6000 - 10000 cP

@Temperature 374 °F
melt, rotational viscometer; DIN 53 019
Evonik Corporation VESTOPLAST® 508 Amorphous Polyalphaolefin
VESTOPLAST 508 is a amorphous polyalphaolefin and butene-rich. Generally used as hot melt adhesives with long open times for the hygiene sector and foam bonding.
Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Cytec (Conap) FR-1050 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Viscosity 6000 - 12000 cP

@Temperature 23.0 °C
6000 - 12000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® H77 Black Thermally Conductive Epoxy
Product Description: EPO-TEK® H77 Black is a two component, thermally conductive, electrically insulating epoxy system designed for lid sealing of hybrids found in hermetic packaging of micro-elect..
Viscosity 6000 - 7000 cP
6000 - 7000 cP
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive
A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc...
Viscosity 6000 cP
6000 cP
Dymax 3094 Solvent-Free Plastic Adhesive
Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide ..
Viscosity 6000 - 7000 cP

@Temperature 35.0 °C
6000 - 7000 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G181 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 6000 cP
6000 cP
ASTM D1824
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, ..
Viscosity 6000 cP
6000 cP
Aremco Crystalbond™ 509 Washaway Mounting Adhesive & Accessory
Provides excellent adhesion and minimizes clogging of diamond tools compared to waxes. Transparent in thin cross-sections. Soluble in acetone or 509-S stripper, an odorless, non-flammable, biodegrad..
Viscosity 6000 - 12000 cP
6000 - 12000 cP
Accelerator
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Viscosity 6000 cP
6000 cP
Mixed; TM R050-12
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..