ChevronTexaco FM Seamer Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name FM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco FM Seamer Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications.This product was developed in consultation with Angelus Sanitary Can Machine Company and key customers.It contains a special biocide to prevent growth of molds when the product comes in contact with water. Chevron Seamer Oil FM provides performance well above that found in typical mineral oils often used in the food industry.ApplicationsChevron Seamer Oil FM is intended for use in food processing industries where incidental food contact may occur.Chevron Seamer Oil FM is engineered to exceed the requirements of and is approved by Angelus Sanitary Can Machine Company for use in the 61H, 62H, 120L, 121L, 140S, and 180S seamers, where an ISO 150 oil is specified. Chevron Seamer Oil FM is intended to extend the machinery`s life to overhaul.Chevron Seamer Oil FM is recommended for:FMC Rotary Cookers and Sterilizers due to its excellent antiwear propertiescirculating systems that require an ISO 150 viscosity due to its excellent low foam properties and oxidation stability.
Physical Properties Metric English Comments
API Gravity 31 °
31 °
Viscosity Measurement 111
111
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 746 SUS
746 SUS
Saybolt Viscosity at 210°F 81.3 SUS
81.3 SUS
Kinematic Viscosity at 40°C (104°F) 143 cSt
143 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 15.4 cSt
15.4 cSt
ASTM D445
Oxidative Stability >= 15000 hour
>= 15000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
Mechanical Properties Metric English Comments
Four Ball Wear 0.560 mm
0.0220 in
Thermal Properties Metric English Comments
Pour Point -9.00 °C
15.8 °F
ASTM D97
Flash Point 284 °C
543 °F
ASTM D92
Descriptive Properties Value Comments
Rust Procedure A, Distilled Water Pass