Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 0.055 ohm | <= 0.055 ohm | at 25 microns thick |
Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental a.. |