Material Notes:
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527
Elongation at Break 20 %
20 %
ISO 527
Elongation at Yield 3.0 %
3.0 %
ISO 527
Tensile Modulus 4.50 GPa
653 ksi
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50N; ISO 306