Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527
Elongation at Break 2.8 %
2.8 %
ISO 527
Tensile Modulus 6.50 GPa
943 ksi
ISO 527
Flexural Strength 165 MPa
23900 psi
ISO 178
Flexural Modulus 4.30 GPa
624 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ISO 75/A
Vicat Softening Point >= 230 °C
>= 446 °F
50N; ISO 306
Copyright © lookpolymers.com All Rights Reserved