Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC AMC™ 2593 (126-40-139) is a carbon fiber reinforced phenolic engineered structural composite molding compound. The carbon fiber is PAN based 3K standard modulus tow. It exhibits outstanding low f.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Loxim 330 01V0 Nylon 6 Information provided by Loxim Industries |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Specific Gravity | 1.55 g/cc @Temperature 23.0 °C |
1.55 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Teknor Apex APEX® 65016 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | Part A |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
E-Polymers SEPAZ® V240A 40% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
BLUESTAR 403HF-G30 PBT, 30% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
E-Polymers SEPAZ® K130HF 30% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | Method A; ASTM D792 |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | Method A; ASTM D792 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |