Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name FLUCON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
80.0 - 100 MPa

@Temperature 1000 °C
11600 - 14500 psi

@Temperature 1830 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.82 - 2.02 W/m-K

@Temperature 1000 °C
12.6 - 14.0 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1000 °C
-0.300 - 0.300 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 82 %
82 %
Fe2O3 1.3 %
1.3 %
SiO2 13 %
13 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2800 kg
Mixing Water 5.5-6 liters
per 100 kgs dry material