Polymer Property : Thermal Conductivity = 1.77 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app..
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app..
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable
Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable
Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable
Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat..
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable
Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat..
Thermal Conductivity 1.77 W/m-K

@Temperature 1100 °C
12.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 60 C Dense Refractory Brick
Description: A bauxite based quality with a high abrasion resistance, successfully used in transition zones of rotary cement kilns.Remarks: This data represents average values, obtained from samples..
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 100 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Thermal Conductivity 1.77 - 1.97 W/m-K

@Temperature 600 °C
12.3 - 13.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Thermal Conductivity 1.77 W/m-K

@Temperature 600.0 °C
12.3 BTU-in/hr-ft²-°F

@Temperature 1112 °F
Stellar Canada CERAMITE® BKR Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..