Mechanical Properties Metric English Comments
Compressive Strength 80.0 - 100 MPa

@Temperature 1000 °C
11600 - 14500 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.