Polymer Property : Compressive Strength = 10900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material
Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 1000 °C
9430 - 10900 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HS Dense Refractory Castable
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable
Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable
Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 13 S Dense Refractory Castable
Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HS Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable
Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable
Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable
Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont..
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable
Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t..