Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material

Category Ceramic , Carbide
Manufacturer Gouda Vuurvast
Trade Name CURAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 3.00 - 5.00 W/m-K

@Temperature 100 °C
20.8 - 34.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
4.00 - 6.00 W/m-K

@Temperature 600 °C
27.8 - 41.6 BTU-in/hr-ft²-°F

@Temperature 1110 °F
5.00 - 7.00 W/m-K

@Temperature 1300 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1300 °C
-0.400 - 0.400 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 18 %
18 %
SiC 70 %
70 %
SiO2 7.0 %
7.0 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2700 kg