Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 4.00 W/m-K @Temperature 650 °C |
27.8 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Thermal Conductivity | 4.00 - 6.00 W/m-K @Temperature 600 °C |
27.8 - 41.6 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c.. |
|||
Thermal Conductivity | 4.00 - 6.00 W/m-K @Temperature 600 °C |
27.8 - 41.6 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |
|||
Thermal Conductivity | 4.00 W/m-K @Temperature 650 °C |
27.8 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 100 Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual.. |
|||
Thermal Conductivity | 4.00 W/m-K @Temperature 2000 °C |
27.8 BTU-in/hr-ft²-°F @Temperature 3630 °F |
|
Touchstone CFOAM® 20 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |