Thermal Properties Metric English Comments
Thermal Conductivity 5.00 W/m-K

@Temperature 100 °C
34.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 98 Dense Refractory Brick
Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 1300 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material
Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 100 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo..
Thermal Conductivity 5.00 W/m-K

@Temperature 100 °C
34.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 1300 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material
Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 100 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1..
Thermal Conductivity 5.00 - 6.00 W/m-K

@Temperature 1400 °C
34.7 - 41.6 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable
Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio..