Polymer Property : Thermal Conductivity = 27.8 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 4.00 W/m-K

@Temperature 650 °C
27.8 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 99 S Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu..
Thermal Conductivity 4.00 - 6.00 W/m-K

@Temperature 600 °C
27.8 - 41.6 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material
Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c..
Thermal Conductivity 4.00 - 6.00 W/m-K

@Temperature 600 °C
27.8 - 41.6 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material
Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b..
Thermal Conductivity 4.00 W/m-K

@Temperature 650 °C
27.8 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast LP 100 Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual..
Thermal Conductivity 4.00 W/m-K

@Temperature 2000 °C
27.8 BTU-in/hr-ft²-°F

@Temperature 3630 °F
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..