Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.00 - 5.00 W/m-K @Temperature 100 °C |
20.8 - 34.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c.. |
|||
Thermal Conductivity | 3.00 - 5.00 W/m-K @Temperature 100 °C |
20.8 - 34.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |