Global GA-3750 High Density Polyethylene, Film Extrusion Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GA-3750 High Density Polyethylene, Film Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsMeets FDA requirements as listed in food additives regulations 21 CFR 177.1520 for use in direct contact with food.Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 0.060 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.060 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 1700 %
1700 %
ASTM D638