Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gichem GIBLEND F70X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blend PC-ABS self-extinguishing class V0 high fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
Izod Impact, Notched 4.50 J/cm
8.43 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 115 °C
239 °F
ASTM D1525/A
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Flammability Test 125
125
[°C] Bilia; IEC 331
Oxygen Index 32 %
32 %
ASTM D2863
Glow Wire Test 960 °C
1760 °F
IEC 695-2-1
Processing Properties Metric English Comments
Middle Barrel Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 100 °C
212 °F
2 hours
Users viewing this material also viewed the following: