Freudenberg Simrit S70 Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Freudenberg Simrit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit S70 Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and biological attack. Avoid chlorinated solvents, aliphatic and aromatic hydrocarbons and petroleum oils. Silicones are generally very permeable to gases and have poor physical strength and abrasion resistance. Typical Uses: LPCVD/Oxidation, Dry Etch, Resist Stripping
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Ultimate 6.90 MPa
1000 psi
Elongation at Break 250 %
250 %
Compression Set 14 %

@Temperature 200 °C,
Time 252000 sec
14 %

@Temperature 392 °F,
Time 70.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Descriptive Properties Value Comments
Color Red