Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature -30.0 °C |
1.80 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature -18.0 °C |
1.80 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar.. |