Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.07 J/cm @Temperature -30.0 °C |
2.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -30.0 °C |
2.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -30.6 °C |
2.00 ft-lb/in @Temperature -23.0 °F |
ASTM D256 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -30.0 °C |
2.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BU00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -30.0 °C |
2.00 ft-lb/in @Temperature -22.0 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifi.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8003 A1 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V T180 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -30.0 °C |
2.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D0850(C) BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 0.000 °C |
2.00 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar.. |