Fiberfil® M-2500 BK Nylon 6, 15% Glass Reinforced, 25% mineral Filled, post industrial

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer FiberFil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® M-2500 BK Nylon 6, 15% Glass Reinforced, 25% mineral Filled, post industrial.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 109.99 MPa
15953 psi
ASTM D638
Flexural Strength 179.99 MPa
26105 psi
ASTM D790
Flexural Modulus 7.000 GPa
1015 ksi
Secant; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D648
Users viewing this material also viewed the following: