Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Various profiles, antishock UV resistant
Physical Properties Metric English Comments
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ISO R 527
Tensile Strength, Yield 39.0 MPa
5660 psi
ISO R527
Elongation at Break 120 %
120 %
ISO R 527
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 78.0 - 80.0 °C

@Load 5.00 kg
172 - 176 °F

@Load 11.0 lb
ISO R306