Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Fainplast Compounds
Trade Name Hax™ HF
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO 1183
Melt Flow 3.5 g/10 min

@Load 21.6 kg,
Temperature 150 °C
3.5 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 41 - 47
41 - 47
ISO 868
Tensile Strength 12.5 MPa
1810 psi
ISO 527
Elongation at Break 230 %
230 %
ISO 527
Thermal Properties Metric English Comments
Oxygen Index 34 %
34 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 100 - 180 °C
212 - 356 °F
extruder
Shelf Life 3.00 Month

@Temperature 30.0 °C
3.00 Month

@Temperature 86.0 °F
Moisture absorption after extended storage