ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS blends for applications where hard/soft combinations are required. The raw materials of this grade are listed in FDA regulations 21 CFR 177.1210 (Closures with sealing gaskets for food containers) and 21 CRF 177.2600 (Rubber articles intended for repeated use), or are considered as generally recognized as safe (GRAS). Also, this grade has passed the end use extraction testing required in these specific regulations for aqueous-based foods only, and it complies with the good manufacturing practices required in 21 CFR 110. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Designed for excellent adhesion onto ABS, PS, PC, PMMA and ASA (cold insert or 2K [two-shot] molding).Recommended for applications requiring superior part surface appearance.Designed for soft touch applications.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
Air at 212°F, 168 hr; ASTM D573
61
61
Air at 257°F, 168 hr; ASTM D573
53

@Thickness 2.00 mm
53

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 1.586 MPa
230.1 psi
Air at 257°F, 168 hr; ASTM D573
2.929 MPa
424.8 psi
Air at 212°F, 168 hr; ASTM D573
4.07 MPa
590 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 1.03 MPa
150 psi
Across Flow; ASTM D412
Elongation at Break 180 %
180 %
Air at 257°F, 168 hr; ASTM D573
516 %
516 %
Air at 212°F, 168 hr; ASTM D573
600 %
600 %
Across Flow; ASTM D412
Compression Set 55 %
55 %
257°F, 70 hr; ASTM D395
Processing Properties Metric English Comments
Melt Temperature 98.9 - 110 °C
210 - 230 °F
For two-shot injection molding
110 - 121 °C
230 - 250 °F
For insertion injection molding
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets