Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.586 MPa | 230.1 psi | Air at 257°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/.. |