Polymer Property : Melt Temperature = 110 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 110 - 310 °C
230 - 590 °F
Average value: 180 °C Grade Count:257
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Melt Temperature 110 °C
230 °F
Processing Temperature
Teknor Apex APEX® 7500-90 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
Melt Temperature 110 - 121 °C
230 - 250 °F
For insertion injection molding
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..
Melt Temperature 110 - 121 °C
230 - 250 °F
For insertion injection molding
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..
Melt Temperature 110 - 120 °C
230 - 248 °F
EMS-Griltech Grilon® KA 115 White CoPA Fiber Count 11
Description: GRILON KA 115 is the low melting homo component fusible adhesive fiber.Data provided by EMS-Griltech.
Melt Temperature 110 - 120 °C
230 - 248 °F
EMS-Griltech Grilon® KA 115 White CoPA Fiber Count 2.2
Description: GRILON KA 115 is the low melting homo component fusible adhesive fiber.Data provided by EMS-Griltech.
Melt Temperature 110 - 120 °C
230 - 248 °F
EMS-Griltech Grilon® KA 115 White CoPA Fiber Count 4.2
Description: GRILON KA 115 is the low melting homo component fusible adhesive fiber.Data provided by EMS-Griltech.
Melt Temperature 110 - 310 °C
230 - 590 °F
Average value: 184 °C Grade Count:538
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..