Material Notes:
Product Description: A nucleated homopolymer resin designed for general-purpose compression molding of articles such as caps and closures. It exhibits excellent strength and high crystallization temperature.Availability: North America Features:Autoclave SterilizableEthylene Oxide SterilizableGood Mold ReleaseHigh SlipLow EmissionsUses: CapsClosuresContainersPackagingPailsRigid PackagingProcessing Method: Compression MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.4 MPa
5420 psi
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1770 MPa
257000 psi
0.05 in/min; ASTM D790A
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
ASTM D648