Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 233 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS E GM30 LE 30% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF15 BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T..
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF40 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GM30 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS WM20 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,..
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p..
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
ASTM D648
ExxonMobil PP1572 Polypropylene Homopolymer
Product Description: A nucleated homopolymer resin designed for general-purpose compression molding of articles such as caps and closures. It exhibits excellent strength and high crystallization te..
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
annealed; ASTM D-648
Axiall ProTherm® 4351 Rigid PVC, Extrusion
Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resi..
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF15 A1 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.