Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1770 MPa | 257000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP1572 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin designed for general-purpose compression molding of articles such as caps and closures. It exhibits excellent strength and high crystallization te.. |